Products | A powerful tool for reducing costs and increasing efficiency in stone production - BYK-W 907 wetting and dispersing agent

Release time:

2021-12-27


Preface
Are you confused about how to improve the wettability of quartz fillers? Are you worried about reducing the total cost of the formulation? Then BYK-W 907 is just in time! BYK-W 907 is a wetting and dispersing agent specially developed for unsaturated resin systems filled with a large amount of quartz sand. Let's learn more about it!


BYK-W 907

Product Overview

Product Description A high molecular weight polymer solution containing filler-friendly groups, with an active substance content of 52%

Usage: 0.25-0.5% based on the liquid component, should be added to the liquid component before adding the filler

Note: Crystallization is likely to occur below 25°C. Heat to 30-40°C before use to clarify the solution.

BYK-W 907 Product Advantages


Reduce the amount of liquid components such as resin

Reduce overall raw material costs

Maintain mechanical properties

Reduce viscosity and increase filler content in casting systems


Specific comparison of product advantages

Reduce the amount of liquid components added

Adding 0.5% of BYK-W 907 to the resin content can reduce the liquid component by 7%.

01

Reduce raw material costs

Adding only 0.5% of BYK-W 907 as a liquid component can reduce the usage of all liquid components by 7%, significantly reducing the overall raw material costs.

02

Maintain mechanical strength

Solution: Increase investment in new product R&D, differentiate design and strive to create popular products

03

Strongly reduces the viscosity of the casting system

Solution: Continue to promote the market, and promote online and offline simultaneously to increase sales

04

Authors' Summary

1. BYK-W 907 can achieve overall cost reduction by reducing the content of liquid components while maintaining its mechanical properties.

2. BYK-W 907 can also reduce the viscosity of the casting system and increase the amount of filler added.
Product Q&A
Q1: For a highly filled casting system, how can the amount of filler added be further increased?
A1: To increase the amount of filler added, the viscosity of the system needs to be reduced. BYK-W 907 can strongly reduce the viscosity of the system and increase the amount of filler added.

Q2: After mixing the quartz stone, I found that there were many dry agglomerated particles. How to solve it?
A2: This is caused by the poor wetting effect of the resin on the quartz sand. BYK-W 907 is recommended to reduce the viscosity of the system and enhance the wetting effect.