Application of Nouryon CC 301 in waterborne wood coatings
Release time:
2022-10-25

CC301
CC 301 is a dispersion with a silica content of 30%. The dispersed silica exists in an amorphous form, commonly known as colloidal silica.
CC 301 has a particle size of 7 nanometers, a uniform particle size distribution, and a large specific surface area. It is a liquid with a specific gravity slightly larger than that of water. Its surface has been modified with silane and has good storage stability.
Applications in water-based wood paint
CC 301 Product Features
01
Significantly improve the hardness of the paint film, improve wear resistance, and have a good surface finish
Preventing adhesion of resin emulsion coatings
Greatly improve the paint film's anti-fouling, chemical corrosion resistance, scrub resistance and water resistance
Improve the adhesion of the paint film, enhance the anti-slip performance of the paint film, and maintain the brightness of the paint film for a long time
Significantly improve the thixotropic properties of the system and enhance the UV and heat aging resistance of the paint film
Improve the conductivity of the paint film and improve the anti-static performance of the paint film
Get the same look and fullness as solvent-based coatings
CC 301 Technical Specifications
02

CC 301 Usage and Dosage
03
The particle size of CC 301 is very small. Compared with traditional colloidal silica, CC 301 can be used at a lower dosage. Different application areas require different dosages and methods. It is recommended to add it to water-based resins and emulsions alone. CC 301 should not be pre-mixed with other additives. The addition amount is usually 10%-40% of the resin or emulsion content (5% to 8% of the total system).
Application in water-based wood coatings
04
Add 10%-40% CC 301 emulsion content to the one-component acrylic formula, and use Momentive silane COATOSIL 2287 (2287 has good storage stability in water-based coatings, and reacts with CC 301 to obtain a denser and more excellent coating) to achieve the same fullness as solvent-based coatings.
Note:
It is recommended to add it directly into the emulsion or resin without premixing with additives.
The addition amount is directly related to the Tg of the resin. A high addition amount is required for a low Tg and a low addition amount is required for a high Tg. Too high an addition amount will result in poor chemical resistance and mechanical properties of the coating.

( END)

Service Hotline:
Focus on us
Contact Information
E-mail:hy@haiyi21cn.com
Address: East Block, 3rd Floor, Mid-term Building, 2000 Zhongshan North Road, Putuo District, Shanghai
Hotline:
400-088-7155
-
E-mail:hy@haiyi21cn.com
Address: East Block, 3rd Floor, Mid-term Building, 2000 Zhongshan North Road, Putuo District, Shanghai
All rights reserved©2022 Shanghai Haiyi Technology & Trade Co., Ltd
The license number for the production and operation of hazardous chemicals is: Shanghai (Feng) Emergency Management Xu [2021]202233(FY)